Hi all,
Just wondering if anyone has had paving done where the grout cracks 4-5 weeks after being layed?
The contractor said there would be an element of cracking but this is literally covering 90% of the 50sqm area.
It is around a fibreglass pool area so understand that due to the wet rainy winter the ground will dry out and could lead to movement however it doesn't seem like enough time to me for that to happen.
They all run linearly along the side of the pavers.
Any thoughts or experience?
Cheers
Phil
Just wondering if anyone has had paving done where the grout cracks 4-5 weeks after being layed?
The contractor said there would be an element of cracking but this is literally covering 90% of the 50sqm area.
It is around a fibreglass pool area so understand that due to the wet rainy winter the ground will dry out and could lead to movement however it doesn't seem like enough time to me for that to happen.
They all run linearly along the side of the pavers.
Any thoughts or experience?
Cheers
Phil
Comment